ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2013, Vol. 34 ›› Issue (3): 34-38.

Previous Articles     Next Articles

Research Progress on Intergranular Corrosion Resistance of Super304H Austenite Stainless Steel

Zhang Chunlei1 , Xiong Xiahua2, Zheng Zhijun2, Zhong Fei1 ,Gao Yan2   

  1. 1 Electric Power Research Institute, Guangdong Power Grid Corp, Guangzhou 510600;
    2 School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640
  • Received:2012-12-26 Online:2013-06-01 Published:2022-09-17

Super304H奥氏体不锈钢晶间腐蚀的研究进展

张春雷1,熊夏华2,郑志军2,钟飞1,高岩2   

  1. 1广东电网公司电力科学研究院,广州510600;
    2华南理工大学材料科学与工程学院,广州510640
  • 作者简介:张春雷(1968-),男,博士,2001年清华大学毕业,电力设备材料和焊接研究。

Abstract: The Super304H austenite stainless steel (0. 10C-18Cr-9Ni-3Cu-0. 4Nb- 0. 08N) is one of first selected materials for superheater and reheater tubes of ultra-supercritical unit. As the steel has higher carbon content and its service temperature ( ~ 650 °C ) is the sensitizing temperature of M23C6 precipitating along grain boundary, how to avoid the occurrence of intergranular corrosion is a main research topic for Super304H steel. The research progress for intergranular corrosion susceptibility of Super304H steel at home and abroad is summarized in this article including intergranular corrosion mechanism, effect of alloy elements in steel especially Nb/C, double solid-solution treatment, stabilizing treatment, welding process and 600 ~ 700 ℃ high temperature aging on intergranular corrosion of this steel, and characterization methods for sensitiveness of intergranular corrosion of Super304H steel. The research and development of Super304H steel is prospected.

摘要: Super304H奥氏体不锈钢(0.10C-18Cr-9Ni-3Cu-0.4Nb-0.08N)为超超临界机组过热器和再热器的首选材料之一,由于该钢含碳较高,服役温度(~650℃)为M23C6沿晶界析出的敏化温度,如何避免晶间腐蚀发生是Super304H钢主要研究课题。本文综述了国内外Super304H钢晶间腐蚀倾向的研究进展,包括晶间腐蚀机理,钢中合金元素特别是Nb/C,双固溶处理、稳定化处理,焊接工艺、600~700℃高温时效对该钢晶间腐蚀的影响和Super304H钢晶间腐蚀敏感性的表征方式。展望了Super304H钢的研究方向。

关键词: Super304H奥氏体不锈钢, 超超临界机组, 晶间腐蚀敏感性, 研究进展