ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2013, Vol. 34 ›› Issue (2): 16-19.

Previous Articles     Next Articles

Progress on Control of Ultra-Low-Oxygen Content and Non-Metallic Inclusions in High Quality Bearing Steel

Yang Hulin1 , He Ping1 , Zhai Yuchun2   

  1. 1. Institute for Metallurgical Process, Central Iron and Steel Research Institute, Beijing 100081;
    2. School of materials and Metallurgy, northeastern University, Shenyang 110004;
  • Received:2012-09-10 Online:2013-04-01 Published:2022-09-30

高品质轴承钢超低氧含量和非金属夹杂物控制的进展

杨虎林1,何平1,翟玉春2   

  1. 1. 钢铁研究总院冶金工艺研究所,北京 100081;
    2. 东北大学材料与冶金学院,沈阳 110004;
  • 作者简介:杨虎林(1986-),男,钢铁研究总院冶金工艺所博士研究生, 精炼理论和工艺技术研究

Abstract: The ultra-low-oxygen content and low rating of inclusions are key indexes for high quality bearing steel. The influence factors on control of ultra-low-oxygen content and nonmetallic inclusions in high quality bearing steel are analyzed including removal of slag during tapping, deoxidation with aluminium, high basicity refining slag, stirring for long time at vacuum or atmosphere, and available process flow sheet. It is obtained that the key factor to produce ultra-clean high quality bearing steel with 5 x 10-6[O] , ≤ 1 x 10-6[ H] and ≤ 12 x 10-6[Ti] is strict control of each steelmaking procedure. The quality of bearing steel produced at home is analyzed and the research orientation for high-quality bearing steel is put forward.

Key words: High-Quality Bearing Steel, Ultra-Low Oxygen, Nonmetallic Inclusion, Steelmaking Process

摘要: 超低氧含量和低夹杂物级别是高品质轴承钢的重要指标。分析了高品质轴承钢中超低氧含量和非金属夹杂物控制的影响因素,如出钢除渣、铝脱氧、高碱度精炼渣、真空或非真空条件下的长时间搅拌和合理的生产工艺流程等。得出生产5×10-6[O]、≤1×10-6[H]和≤12×10-6[Ti]的超纯净高品质轴承钢的关键是对各冶炼工序的严格控制。文中分析了国内轴承钢的质量并提出了研究方向。