Special Steel ›› 2012, Vol. 33 ›› Issue (3): 1-3.

    Next Articles

Water Modeling Test for Auxiliary Deslagging by Blowing Gas in Hot Metal Ladle

Xu Fei1 , Shen Qiaozhen1, Luan Guoqing1 , Wu Zhaohuan1 , Liang Xinliang2, Zhang Xiaowu2 , Yan Jiazhi2   

  1. 1 Key Lab for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081 ;
    2 Lianyuan Iron and Steel Group Co, Loudi 417009
  • Received:2011-11-01 Online:2012-06-01 Published:2022-10-08

铁水罐吹气辅助驱渣水模型实验

许飞1,沈巧珍1,栾国庆1,吴瞾环1,梁新亮2,张小武2,严家志2   

  1. 1武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室,武汉430081 ;
    2涟源钢铁集团公司,娄底417009
  • 作者简介:许飞(1986-),女,硕士研究生,钢铁冶金物理数学模拟。

Abstract: Taking the 90 ~ 105 t hot metal ladle at steel works as prototype, a geometric similarity ratio 1: 4 water model is established in laboratory and the effect of hot metal ladle side-blowing gas for auxiliary-deslagging on skimming area is studied by physical simulation method. Results show that as blowing gas rate is 0.25 〜2.0 m3/h, with increasing gas blowing rate the deslagging area increases ; and with increasing installed angle of porous brick from 0° to 70° and installed height from 174 mm to 294 mm, the deslagging area all increases. With using single porous brick side-blowing to deslag, installed angle 70°, installed height 294 mm and gas blowing rate 0. 8 ~ 1.2 m3/h, the deslagging effect is best.

摘要: 以钢厂90~105 t铁水罐为原型,在实验室建立几何相似比1:4水模型,用物理模拟方法研究铁水罐侧吹辅助扒渣对驱渣面积的影响。结果表明,在吹气流量为0.25~2.0 m3/h时,随着吹气流量的增大驱渣面积增大。同时随着透气砖安装角度从0°到70°、安装高度从174 mm到294 mm时,驱渣面积均会增大。当用单透气砖侧吹驱渣,安装角度为70°,安装高度294 mm,流量为0.8~1.2 m3/h时,驱渣效果最好。

关键词: 铁水罐, 透气砖, 驱渣, 水模型