Behavior of Dynamic Recrystallization of Alloy Tool Steel SKS51

Bao Siqian, Lin Cheng, Zeng Xiangbo, Ding Jinyao, Guo Cun, Zhang Chunyuan   

  1. Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081
  • Received:2012-10-25 Online:2013-04-01 Published:2022-10-08

合金工具钢SKS51的动态再结晶行为

鲍思前,凌程,曾祥波丁晋遥,郭存,张春远   

  1. 武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室,武汉 430081
  • 作者简介:鲍思前(1974-),男,博士,副教授,1996年包头钢铁学院毕业,钢铁材料的组织性能控制、强韧化技术及机理等
  • 基金资助:
    中国博士后科学基金资助项目(No.2012M511282);
    广东省重大科技专项(No. 2010A080407003)

Abstract: The behavior of dynamic recrystallization of alloy tool steel SKS51 (/% : 0.78C, 0.20Si, 0.40Mn, 1.5Ni, 0.30Cr) in single pass hot compression test with strain rate 0.1 ~ 10 s-1 at 850-1 000 ℃ is studied by using Gleeble-1500 thermo-mechanical simulator. Results show that the dynamic recrystallization of steel SKS51 more easily occurs with lower strain rate at higher deformation temperature ; by regression analysis the deformation activation energy and stress exponent of dynamic recrystallization of steel are respectively 336. 97 kJ/mol and 4.26, and based on this foundation the peak strain(εp), stable strain (εs) and critical strain (εc) model are established.

Key words: Alloy Tool Steel SKS51, Single Pass Hot Compression Test, Dynamic Recrystallization, True Stress- True Strain Curves

摘要: 采用Gleeble-1500热模拟机单道次热压缩实验,研究了变形温度850~1 000℃和变形速率0.1~10s-1条件下合金工具钢SKS51(/%:0.78C、0.20Si、0.40Mn、1.5Ni、0.30Cr)的动态再结晶行为。实验结果显示SKS51钢动态再结晶在高的变形温度和低的变形速率情况下更易发生,回归法得出动态再结晶的变形激活能和应力指数分别为336.79 kJ/mol和4.26,并在此基础上建立了动态再结晶峰值应变(εp)、稳态应变(εs)及临界应变(εc)模型。

关键词: 合金工具钢SKS51, 单道次热压缩实验, 动态再结晶, 真应力-真应变曲线