Special Steel ›› 2012, Vol. 33 ›› Issue (3): 53-56.

Previous Articles     Next Articles

Effect of Multi-Stand Pipe Mill Rolling and Sizing Process on Structure and Property of N80 Non-Quenching and Tempering Steel 36-40Mn2V for Oil Well Pipe

Fang Jian1,2, Li Yanghua2, Zou Xiyang2, Xie Kaiyi2, Zhou Yong2, Zhou Mengxiong2, Yuan Zexi1   

  1. 1 Kev Lab for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081 ;
    2 Hengyang Hualing Steel Tube (Group) Co Ltd, Hengyang 421001
  • Received:2011-11-15 Online:2012-06-01 Published:2022-10-14

N80级非调质油井管用钢36-40Mn2V连轧和定径工艺 对组织和性能的影响

方剑1,2,李阳华2,邹喜洋2,谢凯意2,周勇2,周梦雄2,袁泽喜1   

  1. 1武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室,武汉430081 ;
    2衡阳华菱钢管(集团)有限公司,衡阳421001
  • 通讯作者: 袁泽喜,教授,武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室,武汉430081
  • 作者简介:方剑( 1980-),男,博士研究生,工程师,2003年武汉科技大学毕业,钢管产品研发。

Abstract: The effect of 340 multi-stand pipe mill (MPM) continuous rolling process (at 950 ~ 1 100 °C with strain 0. 5 ~ 0. 8, strain rate 1. 0 s _ 1 , water or 3 °C/s cooling) and sizing process ( at 800 ~ 950 °C, with strain 0. 1 ~ 0. 3 , strain rate 0. 5 s -1 , air cooiing) on structure, and hardness of steel 36Mn2V and 40Mn2V has been simulated by using Gleeble-1500 thermal simulation machine. Results show that with MPM deformation temperature being higher than 1 050 °C at strain 0. 5 , the complete dynamic recrystallization of steel 36Mn2V and 40Mn2V occurs, the grains are fine and the comprehensive properties are improved; As sizing strain of steel 36Mn2V is 0. 3 and sizing strain of steel 40Mn2V is 0. 2, as the sizing temperature is controlled higher than 835 °C , the mechanical properties can meet requirement of standard.

Key words: 36Mn2V, 40Mn2V, Non-Quenching and Tempering Steel for Oil Well Pipe, Thermal Simulation, Continuous Rolling, Sizing, Structure, Property

摘要: 通过Gleeble-1500热模拟机,模拟340机组36Mn2V和40Mn2V钢950~1 100℃,变形量0.5~0 8.变形速度1.0 s-1,水冷和3℃/s冷却的连轧工艺与800~950℃,变形量0.10~0.30,变形速度0.5 s-1,空冷的定径工艺对组织和硬度的影响。结果表明,36Mn2V和40Mn2V钢连轧变形温度和变形量分别大于1 050℃和0.5时可发生完全动态再结晶,细化晶粒和提高产品综合性能;36Mn2V钢管定径变形量0.3时,40Mn2V钢定径变形量为0.2时,应控制定径温度大于835℃,才能满足力学性能要求。

关键词: 36Mn2V, 40Mn2V, 非调质油井管用钢, 热模拟, 连轧, 定径, 组织, 性能