An Analysis on Cause of Formation of 0.20C Steel Φ300 mm Round Casting Bloom Intermediate Cracks and Improved Process Measure

Zhang Zhihong1,2 , Liu Jiangwei2 , Zheng Jinfeng2 , Liu Weiping2 , Cheng Guoguang1   

  1. 1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2. Chengde Jianlong Special Steel Co Ltd, Chengde 067201;
  • Received:2011-10-14 Online:2012-04-01 Published:2022-10-14

20钢Φ300 mm圆铸坯中间裂纹成因分析和改善工艺措施

张志宏1,2,刘江伟2,郑锦峰2,刘伟平2,成国光1   

  1. 1. 北京科技大学冶金与生态工程学院,北京 100083;
    2. 承德建龙特殊钢有限公司,承德 067201;
  • 作者简介:张志宏( 1975-),男,博士研究生,1997年包钢钢铁学院毕业,特殊钢开发

Abstract: According to location and morphology of intermediate cracks occurred in macrostructure of 0.20C steel 4>300 mm round casting bloom and combining with analysis on casting equipment and process, it is obtained that with uneven shell thickness formed in mold, larger fluctuation of hydraulic force of withdraw straightening stands on bloom, the intermediate cracks along intergranular boundary form in bloom under action of heat stress and straightening stress. With improving the quality of mold softened water and secondary water for casting, decreasing superheating extent of liquid from 25-35 °C to 20-30 °C , decreasing mold electromagnetic stirring current from 550 A to 350 A, stabling the hydraulic force, and straightening bloom temperature ≥ 950 °C , the intermediate cracks in round casting bloom are eliminated.

Key words: Φ300 mm Casting Round Bloom, Intermediate Cracks, Straightening Force

摘要: 针对20钢φ300mm圆铸坯低倍组织出现中间裂纹的位置和形貌,结合连铸设备和工艺进行分析,得出结晶器内坯壳厚度不均匀,拉矫机矫直压力波动大,铸坯在受到热应力和矫直应力的作用下沿晶界开裂形成中间裂纹。通过改善结晶器软化水和连铸二冷水的质量,钢水过热度由25~35℃降至20~30℃,结晶器电磁搅拌电流由550 A降至350 A,稳定矫直压力,铸坯矫直温度≥950℃,避免了圆铸坯中间裂纹的出现。

关键词: Φ300 mm圆铸坯, 中间裂纹, 矫直力