Special Steel ›› 2012, Vol. 33 ›› Issue (2): 46-48.

Previous Articles     Next Articles

Effect of Forming Pressure on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnet

Zhang Xiaopeng , Yu Xuguang   

  1. Material Institute, Shijiazhuang Railway University, Shijiazhuang 050043
  • Received:2011-09-19 Online:2012-04-01 Published:2022-10-18

成形压力对烧结Nd-Fe-B磁体微观组织与磁性能的影响

张晓鹏,于旭光   

  1. 石家庄铁道大学材料学院,石家庄 050043
  • 作者简介:张晓鹏(1985-),男,硕士研究生(石家庄铁道大学材料学院),2009年河北工业大学毕业,烧结钕铁硼磁体研究

Abstract: The effect of two kinds of forming pressure- 11.54 MPa and 9.23 MPa on microstructure and magnetic properties of Nd-Fe-B magnet has been studied at production line for Φ9. 5 mm sintered Nd-Fe-B magnet (/% : 31.00Pr + Nd, 1.20B, 0.20Al, remainder Fe) manufactured by dry process. Results show that with increasing forming pressure the unevenness of grain size distribution is improved and the grain orientation increases in order to increase remained magnetic induction intensity and magnetic energy product of sintered magnet ; but with increasing forming pressure the grain size increases in order to decrease the intrinsic coercive force of magnet.

Key words: Sintered Nd-Fe-B Magnet, Forming Pressure, Grain Size, Magnetic Properties

摘要: 在于法制备烧结钕铁硼生产线上,研究了11.54 MPa和9.23 MPa两种成形压力对Φ9.5mm烧结钕铁硼磁体(/%:31.00Pr+Nd、1.20B、0.20Al、余Fe)微观组织与磁性能的影响。结果表明,成形压力增大可以改善晶粒分布的不均匀性,提高取向度,从而提高剩磁与磁能积;但成形压力增大易使晶粒尺寸增大,从而使矫顽力降低。

关键词: 烧结钕铁硼, 成形压力, 晶粒尺寸, 磁性能