ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2010, Vol. 31 ›› Issue (1): 12-13.

Previous Articles     Next Articles

Recrystallization Behavior of High Strength Cold Heading Steel SCM435 in Hot Rolling Process

Zhang Yongjun1,2, Han Jingtao1 , Kong Junqi2, Hou Yuehua2, Zheng Yongrui2, Li Jun2 ,Zhen Qinying2   

  1. 1 School of Materials Science and Engineering, University of Science and Technology, Beijing 100083 ;
    2 Xingtai Iron & Steel Corp Ltd, Xingtai 054027
  • Received:2009-08-28 Online:2010-02-01 Published:2022-10-25

SCM435高强冷傲钢热轧过程中的再结晶行为

张永军1,2,韩静涛1, 孔俊其2, 侯月华2, 郑永瑞2, 李军2, 甄琴英2   

  1. 1北京科技大学材料科学与工程学院,北京100083;
    2邢台钢铁有限责任公司,邢台054027
  • 作者简介:张永军(1969-),男,博士后,副教授,钢铁材料生产技术和质量控制。

Abstract: The pass reduction (15% ~70% ) and temperature (850 ~ 1 150 °C ) on recrystallization fraction of tiefor- ming austenite of steel SCM435 (% : 0. 35C, 1. 05Cr, 0. 22Mo) has been studied by using stepped form stock rolling method, and the recrystallization diagram of the steel is got. Results show that with increasing deformation temperature, the critical strain of austenite of steel decreases. The complete recrystallization of austenite of steel SCM435 occurs at 1 150 °C with 45% reduction.

Key words:  , Cold Heading Steel SCM435, Deformation Temperature, Strain, Recrystallization

摘要: 采用阶梯试样轧制法研究了道次变形量(15%~70%)和温度(850~1150℃)对SCM435钢(%:0.35C、1.05Cr、0.22Mo)变形奥氏体再结晶百分比影响,绘制了该钢的再结晶全图。结果表明,随变形温度提高,奥氏体临界变形量降低。在1150℃45%变形量下,SCM435钢奥氏体可以发生完全再结晶。