Development and Application of New Guide Wheel Steel CrllMoV for 550 Mill

Wu Yufeng, Wu Bing, Zhou Yanli, Di Yunfeng , Shi Junqiang   

  1. Special Steel Division, Laiwu Steel Corp Ltd, Laiwu 271105 
  • Received:2012-01-28 Online:2012-08-01 Published:2022-10-25

550轧机新型导轮用钢Crl2MoV的研制与应用

吴玉峰, 吴兵, 周艳丽, 狄云峰, 石军强   

  1. 莱钢股份有限公司特殊钢事业部,莱芜271105
  • 作者简介:吴玉<(1971-),男,工程师,轧钢工艺技术研究与管理。

Abstract: Service life of guide wheel is one of key factors to influence the size precision of rolled products. With practice of φ70 mm 20CrMnTiH gear steel product by 550 mill, according to test of properties of 4 steel grade- T8, Crl6Ni3, Crl2MoV and Cr23Ni5Mo for guide wheel and effect of different heat treatment processes on service life of 670 mm guide wheel, the steel Crl2MoV (/%: 1. 45 - 1. 55C, ≤0.60Si, ≤ 0.60Mn, 12. 00 ~ 13.00Cr, 0. 90 ~ 1.10Mo, 0.90 ~ 1.10V) with fining carbide heat treatment and final cold treatment is selected as guide wheel material, the service life of guide wheel made of steel Crl2MoV is up to 2 000 t, it is available to ensure size precision and decrease reject.

Key words:  , 550 Mill, Guide Wheel, Steel Cr12MoV, Development

摘要: 导卫导轮的使用寿命是影响轧材尺寸精度的重要因素。通过550轧机生产φ70 mm 20CrMnTiH齿轮钢的实践,根据4种导轮用钢T8、Cr16Ni3、Cr12MoV、Cr23Ni5Mo的性能试验和不同热处理工艺对φ70 mm导轮使用寿命的影响,优选了Cr12MoV钢(/%:1.45~1.55C、≤0.60Si、≤0.60Mn、12.00~13.00Cr、0.90~1.10Mo、0.90~1.10V)作为导轮材料并进行细化碳化物热处理和最终冷处理工艺,使Cr12MoV钢制成的导轮使用寿命达2 000 t,有效地保证钢材高精度轧制,减少尺寸废品。