A Discussion on Progress of Domestic Electric Arc Furnace Steelmaking Technology

Li Shiqi1, Sun Hua1,2, Yu Jian1 , Pei Fen1   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 Nanjing Iron and Steel Corporation, Nanjing 210035
  • Received:2010-05-06 Online:2010-12-01 Published:2022-10-27

我国电弧炉炼钢技术的进展讨论

李士琦1,孙华1,2,郁健1,裴芬1   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2南京钢铁联合有限公司,南京210035
  • 作者简介:李士琦(1942-),男,教授,《特殊钢》编委,电弧炉炼钢、特 殊钢冶炼和精炼、冶金反应工程及过程控制研究。

Abstract: Domestic electric arc furnace steelmaking technology including output, equipment technique (large-capacity, advanced eccnomic and technic index), high efficiency technology (ultra-high power supply, auxiliary energy source, diversified charging, decreasing power off-time, scrap preheat and continuous smelting) and cleanliness technology has been gained obvious progress in last decade. But the factors such as shortage of scrap source, power in short supply and unreasonable energy structure restrict the further development of domestic electric arc furnace steelmaking. The focal points for development of domestic electric arc furnace steelmaking (diversified charging, reasonable power supply , energy multiplicity ,residual heat utilization and green environmental protection) and forward progress (clean steel production for low carbon economic) have been discussed in article.

Key words: Domestic Electric Arc Furnace Steelmaking, Technology, Progress

摘要: 10年来我国电弧炉炼钢技术在产量、装备技术(大型化、高的技术经济指标)、高效化技术(超高功率供电、辅助能源、炉料多元化、减少非通电时间、废钢预热、连续化生产)和洁净化技术方面均取得了显著进展。但是废钢资源短缺、电力不足和能源结构不合理等因素制约了我国电弧炉炼钢的进一步发展。文中讨论了我国电弧炉炼钢发展的重点(炉料多样化、合理供电、能量多样化、余热利用和绿色环保)和前瞻(低碳经济洁净钢生产)。

关键词: 我国电弧炉炼钢, 技术, 进展