A Study on Non-Carbon Steelmaking at High Temperature
Hou Mingshan1 , Fan Xinyou2 , Liu Chao1 , Dong Hongbo1 , Li Shiqi1
1. Metallurgical and Ecological Engineering School, University of Science and Technology, Beijing 100083 ;
2. Xinxing Ductile Iron Pipe Co Ltd, Wu,an 056300
Hou Mingshan , Fan Xinyou , Liu Chao , Dong Hongbo , Li Shiqi. A Study on Non-Carbon Steelmaking at High Temperature[J]. Special Steel, 2011, 32(5): 14-17.