Designing Characteristics of Annealing and Pickling Line for 16 mm Hot Rolled Stainless Steel Strips

Xu Yuanjun , Li Chunming   

  1. Zhongye Southern Engineering and Technology Co Ltd, Wuhan 430223
  • Received:2011-03-22 Online:2011-10-01 Published:2022-11-02

16 mm热轧不锈钢带退火酸洗生产线的设计特点

徐远军,李春明   

  1. 中冶南方工程技术有限公司,武汉 43022
  • 作者简介:徐远军(1981-),男,硕士,工程师,2007年武汉科技大学毕业,冷轧工艺设计。

Abstract: The process flow sheet, key equipment and technology characteristics for maximum coil weight 35 t, 2 ~ 16 mm hot rolled stainless steel strip annealing and pickling line are presented. The steel grades produced in the line are austenite ,ferrite and martensite stainless steel; the strip is heated in annealing furnace by natural gas, the furnace temperature is up to 1 180 °C and the total furnace length is 96 m; the effective descaling is carried out before pickling, the pickling solutions are sulphuric acid and nitric acid + hydrofluoric acid, the maximum speed of pickling is 60 m/min, the waste water and waste acid are recovered and regenerated, and the acid mist are also recovered and treated.

Key words: Hot Rolled, Stainless Strip, Annealing, Pickling

摘要: 介绍了最大卷重35 t、2~16 mm热轧不锈钢带退火酸洗线的工艺流程、关键设备和技术特点。该机组所生产的钢种有奥氏体、铁素体和马氏体不锈钢;退火炉使用天然气加热钢带,炉温可达1180℃,炉子总长96m;在酸洗前进行有效除鳞,酸洗的溶液为硫酸,硝酸+氢氟酸,酸洗最大速度为60 m/min,废水和废酸经回收再利用,酸雾经回收和处理。

关键词: 热轧, 不锈钢带, 退火, 酸洗