Reutilization of 80 t LF Hot Return Reflning Slag for Special Steel

Ding Ning1,2, Qin Dengping2, Wang Jian2, Bao Yanping2, Wang Lifeng2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 Research Institute of Technology, Shougang, Beijing 100043
  • Received:2011-03-09 Online:2011-08-01 Published:2022-11-03

80 tLF精炼特殊钢的热态返回渣的循环应用

丁宁1,2, 秦登平2,王坚2,包燕平2,王立峰2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2首钢技术研究院,北京100043
  • 作者简介:丁 宁(1979-),男,硕士,工程师,2007年东北大学毕业,品种钢的开发。

Abstract: The LF hot return slag process at Shougang is reutilized to refine steels including steel 82B, 40Cr, 20CrMnTi and 60Si2Mn. During refining special steels in LF with using hot reducing return slag, 200 〜400 kg/heat of synthetic slag or active lime is added, the consumption of calcium carbide increases properly, and the slag is deoxidized by aluminum shot, calcium carbide and silico-ferrite powder. Production practice shows that with using this process the refining desulphurization rate is more than 50%, after LF refining the liquid oxygen activity ≤ 10 x 10 -6, the LF slag making materials- synthetic slag decreases by 5kg/t steel and submerged arc slag decreases by 2 kg/t steel, and the melting cost decreases by 7 yuan/1 steel. The hot refining slag has higher reutilization value.

Key words:  , LF, Hot Refining Slag, Reutilization

摘要: 首钢精炼82B、40Cr、20CrMnTi、60Si2Mn等钢种采用LF循环利用热态返回渣工艺。LF使用热态还原循环渣精炼特殊钢时,补加合成渣(或活性石灰)200~400kg/炉,适当增加电石消耗量,并用铝粒、电石、硅铁粉对渣脱氧。生产实践表明,采用该工艺使精炼脱硫率达到50%以上,LF后钢水氧活度≤10×10-6,并使LF造渣料-合成渣减少5kg/t钢,埋弧渣减少2kg/t钢,冶炼成本降低7元/t钢。热态精炼渣具有较高的回收利用价值。