Effect of Nitrogen Content on Behavior of High Temperature Deformation of Crl2N Alloy

Yang Jichun , Liu Nan   

  1. School of Material and Metallurgy, Inner Mongolia University of Science and Technology, Baotou 014010
  • Received:2011-03-09 Online:2011-08-01 Published:2022-11-03

氮含量对Crl2N合金高温形变行为的影响

杨吉春, 刘南   

  1. 内蒙古科技大学材料与冶金学院,包头014010
  • 作者简介:杨吉春(1963-),男,博士,教授,硕士生导师,1984年包头钢铁学院毕业,稀土在钢中应用研究。

Abstract: Cr12N alloy (% : 2. 03 〜2.26C, 0. 16 〜0. 33Si, 0. 29 ~0. 37Mn, 11. 86 〜11.96Cr, 0. 09 〜0. 28N) is melted by a 10 kg vacuum induction furnace with N-alloying by filling nitrogen and adding silicon nitride. The Crl2N alloys bearing different N content are heated to 1 180 for 3 min with 10 °C/s at vacuum, then cooled to 1 100 ~900 °C for 20 s with 10 °C/s and compressed by 30% with 1 ~ 10%" by using a Gleeble-1500 thermo-mechanical simulation machine to get the true stress-strain curves and the effect of nitrogen on mechanical properties of the alloy at high temperature. Results show that N inhibits occurrence of dynamic recrystallization of alloy ; as deformation at high temperature the dynamic recovery is dominating softening mechanism of the Crl2N alloy; and as compared with 0. 09% N alloy and 0. 28% N alloy, the 0. 18% N alloy has higher peak stress and yield stress, and its recovery activation energy is lowest.

Key words:  , Cr12N Alloy, N, High Temperature Deformation, Dynamic Recovery

摘要: Cr12N合金(%:2.03~2.26C、0.16~0.33Si、0.29~0.37Mn、11.86~11.96Cr、0.09~0.28N)由10kg真空感应炉熔炼并通过充氮和加氮化硅进行N合金化。通过Gleeble-1500热模拟试验机将不同N含量的Cr12N合金在真空下以10℃/s加热至1180℃3min,再以10℃/s冷却至1100~900℃20s,以1~10~2s-1进行30%压缩变形,得出真应力-应变曲线和氮对该合金高温力学性能的影响。结果表明,N抑制合金动态再结晶发生,Cr12N合金在高温变形时,动态回复是最主要的软化机制;与0.09%N合金和0.28%N合金比较,0.18%N合金具有较高的峰值应力和屈服应力,回复激活能最低。