ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2010, Vol. 31 ›› Issue (3): 62-64.

Previous Articles     Next Articles

Effect of Annealing Process and Cold Rolling Reduction on Texture of CSP Thin Sheet of Ultra-low Carbon Steel

Liu Haixia, Wang Baokun , Jin Zili   

  1. Material and Metallurgy School, Inner Mongolia University of Science and Technology, Baotou 014010
  • Received:2009-12-01 Online:2010-06-01 Published:2022-11-07

退火工艺及压下率对超低碳CSP冷轧薄板织构的影响

刘海霞,王宝昆,金自力   

  1. 内蒙古科技大学材料与冶金学院,包头014010
  • 通讯作者: 金自力
  • 作者简介:刘海霞(1982-),女,硕士研究生,深冲板的冷轧织构研究。
  • 基金资助:
    国家自然科学基金项目(50761005)、内蒙古自然科 学基金项目(20080404Zd18)资助

Abstract: The hood type furnace annealing process at 700 °C of 1.9 mm and 1.0 mm thin sheet cold rolled with 62. 0% and 71.4% reduction of ultra-low carbon steel DC01 ( 0. 047% C ) and SPCC (0. 041 % C ) produced by CSP process at Baotou Iron and Steel Co has been simulated in laboratory by electric resistance furnace. Results show that the main textures of annealed cold rolling sheet are {111}〈110〉and {111}〈112〉 ; the orientation density of {112}〈110〉 in cold rolling sheet with reduction 71.4% annealed with faster heating rate is greatest, the proportion of large-angle grain boundary is larger, the density of textures is higher and the texture mainly concentrates near the -y orientation fibre.

摘要: 在实验室用电阻炉模拟了包钢CSP工艺生产的以62.0%和71.4%压下率冷轧的1.9 mm和1.0 mmCD01钢(0.047%C)和SPCC钢(0.041%C)冷轧板的700℃罩式退火工艺。结果表明,冷轧板退火后主要以{111}〈110〉和{111}〈112〉织构为主;71.4%压下率冷轧板快速升温退火后{112}〈110〉取向密度最大,且大角度晶界所占比例较大,织构密度较大,织构主要集中在γ取向线附近。