ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (6): 10-13.

Previous Articles     Next Articles

Recent Progress on Electroslag Remelting Technology

Jiang Zhouhua1,Li Zhengbang2   

  1. 1 School of Materials and Metallurgy, Northeastern University, Shenyang 110004;
    2 Central Iron and Steel Research Institute, Beijing 100081
  • Received:2009-05-26 Online:2009-12-01 Published:2022-11-14

电渣冶金技术的最新发展趋势

姜周华1,李正邦2   

  1. 1东北大学材料与冶金学院,沈阳110004;
    2北京钢铁研究总院.北京100081
  • 作者简介:姜周华(1963-),男,博士,教授,《特殊钢》编委,特殊冶炼工艺理论研究。 李正邦( 1934-),男,教授,中国工程院院士,《特殊钢》特邀编委,特种冶金和二次精炼、高温合金和特种钢研究。

Abstract: The development history of electroslag remelting ( ESR) commercial production for 50 years is reviewed briefly, and the presentation and evaluation of new technology of ESR metallurgy in recent years are focused including electroslag rapid remelting, double electrode series electroslag continuous casting technology, ultra-heavy slab ingot ESR, technology for solidification segregation control of heavy ESR ingot, ESR furnace with controlled atmosphere and ESR casting technology with liquid metal. It is indicated that in new development phase the ESR metallurgical technology is developed with high efficiency, saving energy, environmental protection and meeting requirement for higher quality.

摘要: 简要回顾了电渣重熔工业生产50年的发展历史,重点对近年来电渣冶金新技术进行了介绍和评价,包括快速电渣重熔,双极串联电渣连铸技术,特厚板坯电渣重熔,大型电渣重熔钢锭凝固偏析控制,可控气氛电渣炉和电渣液态浇铸技术。在新的发展阶段,电渣冶金技术向高效、节能、环保和满足更高质量方向发展。