An Analysis on Solubility Products for Ti Inclusions in Austenite of Low Carbon Steels

Qi Haiquan1,2, Yong Qilong2, Yong Xi2,3 , Chen Mingxin2   

  1. 1 Faculty of Mechanical and Electrical Engineering, Kunming University of Science and Technology, Kunming 650093 ;
    2 Central Iron and Steel Research Institute, Beijing 100081 ;
    3 Institute of Computing Technology, Chinese Academy of Science, Beijing 100190
  • Received:2009-08-31 Online:2010-04-01 Published:2022-11-15

低碳钢奥氏体中Ti夹杂溶解度积的分析

亓海全1,2, 雍岐龙2, 雍兮2,3, 陈明昕2   

  1. 1昆明理工大学机电学院,昆明650093;
    2钢铁研究总院,北京100081;
    3中科院计算所,北京100190
  • 作者简介:亓海全(1981-),男,博士,微合金钢研究。

Abstract: Solubility products for Ti inclusions in austenite of low carbon steels (including interstitial free - IF steel) have been calculated and compared qualitatively. Results show that without considering effect of other factors, at 950 ~ 1 250 ℃ , the TiN has minimum solubility product and the TiC has maximum solubility product while that of TiS and Ti4C2S2 are mediums. It indicates that at high temperature the initial precipitate should be TiN, then TiS, Ti4C2S2, and last TiC.

Key words: Low Carbon Steel, Austenite, Ti Inclusions, Solubility

摘要: 对低碳钢(含无间隙原子-IF钢)奥氏体中Ti的各类夹杂物固溶度积进行了计算和定性比较。结果表明,在不考虑其它因素影响的情况下,在950~1 250℃,TiN具有最小的固溶度积,TiC具有最大的固溶度积,而TiS和Ti4C2S2则处其间。表明低碳钢在高温时优先析出的应该是TiN,其次是TiS和Ti4C2S2,而TiC析出则处在最后。