Development of Nb Microalloying High Strength Ship Plate at Anyang Steel

Zhu Hongyi   

  1. Anyang Iron and Steel Co Ltd, Anyang 455004
  • Received:2008-11-24 Online:2009-06-01 Published:2022-11-24

安钢Nb微合金化高强度船体结构钢板的开发

朱红一   

  1. 安阳钢铁股份有限公司、安阳455004
  • 作者简介:朱红一(I960-),男,高级工程师,副总机械师,1982年北京科技大学毕业,中厚板生产技术管理。

Abstract: Nb microalloying high strength ship plate was produced by 100 t converter-100 t LF-200 mm x 1 500 mm caster-2800 mm medium plate mill flow sheet at Anyang Steel. Production data statistic results showed that with precisely controlling chemical composition of steel ( % : 0. 13 ~0. 16C, 0. 33 ~0. 43Si, 1. 31 ~ 1.42Mn, 0. 007 〜0. 014P, 0. 005 〜 0. 018S, 0. 021 ~0. 039Al, 0. 018 -0. 022Nb) , beginning finish rolling at 950 °C , total reducing ≥50% in finish rolling, and end finish rolling at 780 ~ 850 °C , the grain size rating of 6 〜25 mm steel plate of grade AH36 was 9 ~ 9. 5, yield strength 360 ~475 MPa, tensile strength 490 〜610 MPa, 85 elongation 18% 〜36% and impact energy at 0°C 110 〜221 J.

Key words: Nb Microalloying, High Strength Plate, Control Rolling

摘要: 安阳钢铁公司通过100 t转炉-100 t LF-200 mm×1 500 mm连铸机-2800 mm中板轧机生产流程开发了Nb微合金化高强度船板。生产数据统计结果表明,通过精确控制钢的成分(%:0.13~0.16C、0.33~0.43Si、1.31~1.42Mn、0.007~0.014P、0.005~0.0185、0.021~0.039A1、0.018~0.022Nb),精轧开始温度950℃,精轧累积压下率≥50%,终轧温度780~850℃,使AH36牌号6~25 mm钢板的晶粒度为9~9.5级,屈服强度360~475 MPa,抗拉强度490~610 MPa,δ5伸长率18%~36%,0℃冲击功110~221J。

关键词: Nb微合金化, 高强度钢板, 控制轧制