ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (3): 58-60.

Previous Articles     Next Articles

Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N

Wang Xiaofeng1 , Chen Weiqing1 , Bi Hongyun2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 Baosteel Co Ltd, Shanghai 201900
  • Received:2008-11-15 Online:2009-06-01 Published:2022-11-24

固溶处理对00Cr25Ni7Mo4N双相不锈钢组织和力学性能的影响

王晓峰1, 陈伟庆1, 毕洪运2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2宝山钢铁股份有限公司,上海201900
  • 作者简介:王晓峰(1979-),男,博士研究生.钢的质量硏究与品种开发

Abstract: Effect of phase proportion and solution temperature on structure and mechanical properties of steel 00Cr25Ni7Mo4N ( % : 0. 007 ~0.009C, 24. 50 〜24. 84Cr, 6.92 〜6.99Ni, 3.65 〜3. 72Mo, 0. 27 ~0. 30N) melted by vacuum induction furnace (6. 5 kg ingot) has been studied. Results showed that with increasing solution temperature from 1 050 °C to 1 200 °C , ferrite content in steel increased from 48% 〜50% to 53% 〜55% ; with increasing solution temperature from 1 050 °C to 1 100 °C , the strength of steel decreased while the elongation and impact toughness of steel increased ,and with increasing the solution temperature from 1 100 °C to 1 200 °C , the strength of steel increased while the e- longation and impact toughness of steel decreased, so optimum temperature of the steel was 1 100 °C ±50°C.

Key words: Duplex Stainless Steel 00Cr25Ni7Mo4N, Phase Proportion, Solution Temperature, Mechanical Properties

摘要: 研究了真空感应炉(6.5 kg锭)熔炼的00Cr25Ni7Mo4N钢(%:0.007~0.009C、24.50~24.84Cr、6.92~6.99Ni、3.65~3.72Mo、0.27~0.30N)的相比例和固溶处理温度对钢的组织和力学性能的影响。结果表明,随固溶温度由1 050℃增至1 200℃,钢中铁素体含量由48%~50%提高至53%~55%。当固溶温度由1 050℃提高至1100℃,钢的强度下降,伸长率和冲击韧性增加,当固溶温度由1 100℃提高至1 200℃,钢的强度增加,伸长率和韧性降低,该钢最佳固溶温度为1 100℃±50℃。