Zou Yong , Sun Mingshan. Denitriding Process for Ultra-pure Ferrite Stainless Steel in
85 t VOD Refining and Its Effect[J]. Special Steel, 2009, 30(6): 39-41.
邹勇, 孙铭山. 85 t VOD精炼超纯铁素体不锈钢的脱氮工艺及效果[J]. 特殊钢, 2009, 30(6): 39-41.
1Pehlke R D, Elliott J F. Solubility of Nitrogen in Liquid Iron Alloys. Transactions of the Metallurgical Society of AIME, 1960 ,218 : 1088
2Humber J C, Elliott J F. The Solubility of Nitrogen in Liquid Fe-Cr-Ni Alloys. Transactions of the Metallurgical Society of AIME, 1960,218 : 1076
3Chipman J, Corrigan D A. Prediction of the Solubility of Nitrogen in Molten Steel. Transactions of lhe Metallurgical Society of AIME, 1965,233:1249
4黄希祜.钢铁冶金原理.第2版.北京:冶金工业出版社,1990
5陈国光.真空下钢液脱氮工艺研究.钢铁,1999,34(1):17