ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (6): 49-51.

Previous Articles     Next Articles

Effect of Ti-Nb on Formability of Annealed Cold Rolled Sheet of Ultra-Low Carbon Ferrite Stainless Steel Cr18

Sun Dan1 , Chen Weiqing1 , He Shen2, Shen Jicheng2 ,Zheng Hongguang2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2 Technology Center Stainless Steel, Baosteel Institute, Shanghai 201900
  • Received:2009-05-13 Online:2009-12-01 Published:2022-11-29

Ti-Nb对Cr18超低碳铁素体不锈钢冷轧板成形性能的影响

孙丹1,陈伟庆1,何慎2,沈继程2,郑宏光2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2宝钢研究院不锈钢技术中心,上海201900
  • 通讯作者: 陈伟庆
  • 作者简介:孙丹(1982-),女,硕上研究生,铁素体不锈钢织构和成形性能研究。

Abstract: Effect of 0 ~ 0. 21 % Ti and 0 ~0. 29% Nb on structure, recrystallization texture, mechanical properties and formabilitv of ultra-low carbon ferrite stainless steel Cr18 (% : 0. 008 ~0. 009C, 17. 48 ~ 17. 57Cr) has been studied. Results show that the grain size of annealed cold rolled sheet of Nb stabilized steel is finer than that of Ti stabilized steel; the {111} < 112 > orientation density of cold-rolled sheet by Ti-Nb stabilization is maximum, that by Ti stabilization is second and that by Nb stabilization is minimum; the strain-hardening exponent n- value of annealed cold-rolled sheet by Ti, Nb and Ti-Nb stabilization is respectively 1. 55, 1. 12 and 1.48, therefore the formability of annealed cold-rolled sheet by Ti and Ti-Nb stabilization is excellent.

Key words: Ti-Nb, Ferrite Stainless Steel Cr18, Texture, Formability

摘要: 研究了0~0.21%Ti和0~0.29%Nb对Cr18钢(%:0.008~0.009C、17.48~17.57Cr)的组织、再结晶织构、力学性能和成形性能的影响。结果表明,Nb稳定化退火冷轧板的晶粒较Ti稳定化退火冷轧板细小;Ti-Nb稳定化的冷轧板{111}〈112〉取向密度最大、Ti稳定化冷轧板次之,Nb稳定化冷轧板最小;Ti、Nb、Ti-Nb稳定化退火冷轧板应变硬化指数n值分别为1.55、1.12和1.48,因此Ti和Ti-Nb稳定化退火冷轧板的成形性良好。