Development and Application Prospects for Hot Rolled Steel Sheet Piles

Ren Anchao1,2, Zhou Guifeng1,2, Ji Yu1, Zhu Min1   

  1. 1 Research and Development Institute, Wuhan Iron and Steel ( Group) Corp, Wuhan 430080;
    2 Institue of Material Science and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081
  • Received:2008-07-14 Online:2009-02-01 Published:2022-11-29

热轧钢板桩的发展和应用前景

任安超1,2, 周桂峰1,2, 吉玉1, 朱敏1   

  1. 1武汉钢铁(集团)公司研究院,武汉430080;
    2武汉科技大学材料科学与冶金学院,武汉430081
  • 作者简介:任安超(1976-),男,博士在读,工程师,高性能型钢研究
  • 基金资助:
    武汉市科技计划资助项目(20061002085)

Abstract: Sheet piles are new environmental-protection construct steel products which wide apply in the fields such as wharf, dock, pier, dyke, embankment, retaining wal] and weir projects. The sheet piles have many advantages including high strength, light, waterproof, strong endurance, obvious environmental-protection effect, construction simplicity, strong function for rush to deal with an emergency (a breach in an embankment) etc. The development, engineering application, standard and market prospects in China are analyzed.

Key words: Hot Rolled Steel Sheet Piles, Application, Development

摘要: 钢板桩是一种新型环保建筑钢材,广泛应用于码头、堤防护岸、挡土墙、船坞、围堰等工程。钢板桩具有高强度、轻型、隔水性好、耐久性强、环保效果显著,施工简单,较强的救灾抢险功能等优点。分析了我国热轧钢板的发展,工程应用、标准以及市场前景。

关键词: 热轧钢板桩, 应用, 发展