Effect of Nb on Oxidation Resistance and High Temperature Tensile Strength of As-cast Alloy HP40

Yang Liang1 , Zhang Jinlong1,2, Zhao Tuan1 , Wu Wenxia3, Gao Zhanyong1   

  1. 1 Material and Metallurgy School, Inner Mongolia University of Science and Technology, Baotou 014010;
    2 General Machinery Company, Baogang Group, Baotou 014010;
    3 Inner Mongolia Wulanchabu Vocational College, Wulanchabu 012000
  • Received:2009-05-21 Online:2009-12-01 Published:2022-11-30

Nb对铸态HP40合金抗氧化及高温强度的影响

杨亮1,张金龙1,2,赵团1,武文霞3,高占勇1   

  1. 1内蒙古科技大学材料与冶金学院,包头 14010;
    2包钢机械综合公司,包头014010;
    3内蒙占乌兰察布职业学院,乌兰察布012000
  • 通讯作者: 高占勇
  • 作者简介:杨亮(1979-),男,助理工程师,内蒙古科技大学毕业,微合金钢和高温合金研究。

Abstract: Effect of Nb content on oxidation resistance and tensile strength at 1 150 T of as-cast alloy HP40 ( % : 0. 40C, 25Cr, 35Ni, 0. 15Mo, 0. 05Ti, 0. 4 〜2. 1 Nb) melted by a 10 kg vacuum induction furnace has been studied by Gleeble-1500 thermal simulation machine. Results show that the HP40 alloy contained 0. 8% Nb has excellent comprehensive high temperature properties that is at 1 150 ℃ , the oxidation weight gain- 0. 766 g/( m2·h) is lowest and the tensile strength (52 MPa) is highest.

Key words: Nb, Alloy HP40, Oxidation Resistance, High Temperature Strength

摘要: 通过Gleeble-1500热模拟机研究了Nb含量对10 kg真空感应炉熔炼的铸态HP40合金(%:0.40C、25Cr、35Ni、0.15Mo、0.05Ti、0.4~2.1Nb)1 150℃抗氧化性和抗拉强度的影响。结果表明,0.8%Nb时,HP40合金具有最佳的综合高温性能:在1 150℃合金氧化增重最低,为0.766 g/(m2·h),抗拉强度最高,为52 MPa。

关键词: Nb, HP40合金, 抗氧化性, 高温强度