Special Steel ›› 2008, Vol. 29 ›› Issue (1): 43-44.
Previous Articles Next Articles
Zhao Hongyan
Received:
Online:
Published:
赵鸿燕
作者简介:
Abstract: The adding nitrogen processes by added nitrided ferrochrome (56. 2%Cr, 7. 33% N) with (0. 1 ~0. 6) x 105 Pa argon or nitrogen atmosphere in 200 kg vacuum induction furnace for melting nitrogenous stainless steel Crl3 (0. 04% ~0.06%N), Cr23Nil9 (0. 22% 〜0.28%N) and Cr22Ni9 (0. 15% ~0. 19%N) have been tested and studied. Results showed that with added nitride alloy in nitrogen atmosphere the yield of nitrogen was more than 80% , while with added nitride alloy in argon atmosphere the yield of nitrogen only 10%. With increasing nitrogen pressure in furnace, controlling suitable adding temperature and adding smaller size nitride ferrochrome, the yield of nitrogen was up to 100%.
Key words: Vacuum Induction Furnace, Nitrogenous Stainless Steel, Nitrogen Atmosphere, Nitride Ferrochrome, Yield of Nitrogen
摘要: 试验研究了200 kg真空感应炉冶炼含氮不锈钢Cr13(0.04%~0.06%N)、Cr23Ni19(0.22%~0.28% N)和Cr22Ni9(0.15%~0.19%N)时,在(0.1~0.6)×105Pa氩气或氮气下加氮化铬(56.2%Cr、7.33%N)增氮工艺。结果表明,在氮气保护下加氮化合金,氮回收率为80%以上;在氩气保护下加氮化合金,氮回收率仅为10%。提高炉内氮气压力,控制合适的加入温度,加入小粒度氮化铬,氮的回收率可达100%。
关键词: 真空感应炉, 含氮不锈钢, 氮气保护, 氮化铬, 氮回收率
Zhao Hongyan. Adding Nitrogen Process by Alloy for Melting Nitrogenous Stainless Steels in Vacuum Induction Furnace[J]. Special Steel, 2008, 29(1): 43-44.
赵鸿燕. 真空感应炉冶炼含氮不锈钢的合金增氮工艺[J]. 特殊钢, 2008, 29(1): 43-44.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2008/V29/I1/43