ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2008, Vol. 29 ›› Issue (3): 42-43.

Previous Articles     Next Articles

Analysis on Key Producing Process of Super304H Steel Tube for Ultra-Supercritical Electric Power Unit

Peng Fangfang1, Zhu Guoliang2, Song Jianxin2   

  1. 1 Material Institute,Dongfang boiler(Group)Co Ltd,Zigong 643001;
    2 Jiangsu Wujin Stainless Steel Pipe Plant Co Ltd,Changzhou 213111
  • Received:2007-11-10 Online:2008-06-01 Published:2022-12-22

超(超)临界发电机组用Super304H钢管关键制造工艺的分析

彭芳芳1, 朱国良2, 宋建新3   

  1. 1东方锅炉(集团)股份有限公司材料研究所,自贡643001;
    2江苏武进不锈钢管厂集团有限公司,常州213111
  • 作者简介:彭芳芳(1957-),女,高级工程师,所长,1982年西安理工大 学毕业,锅炉材料研究。

Abstract: With analysis on producing process and quality of Super304H(0.07~0. 13C,17.0~19.0Cr,7.5~ 10.5Ni,0.001~0.010B,0.3~0.6Nb,2.5~3.5Cu,0.05~0. 12N)steel tube for more than 600 MW ultra- supercriti- cal electric power unit made at home and abroad, it is obtained that in order to get better high temperature mechanical prop- erties and corrosion resistance,the optimum chemical composition control is ≤0.08C,≤3.0Cu,0.0002S,Nb/C≥5, Nb/(C+N)≥2.The key processes such as heat treatment,cold working deformation and shot peening for Super304H steel tube are presented in this article.

摘要: 通过对国内外制造的600 MW以上的超(超)临界发电机组用Super304H钢(%:0.07~0.13C、17.0~19.0Cr、7.5~10.5Ni、0.001~0.010B、0.3~0.6Nb、2.5~3.5Cu、0.05~0.12N)管材的制造工艺和质量分析,得出为获得较好的高温力学性能和耐腐蚀性,最佳的成分控制为:≤0.08%C、≤3.0%Cu、0.0002%S、Nb/C≥5、Nb/(C+N)≥2。文中叙述了Super304H钢管的热处理,冷加工变形量,喷丸等关键工艺。