ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2008, Vol. 29 ›› Issue (3): 60-62.

Previous Articles     Next Articles

Research and Production of a Low Carbon Bainitic Steel XDB685 at Xiangtan Steel

Xia Zhenghai, Cao Bo,   Cao Zhiqiang   

  1. R&D Center,Xiangian lron and Stel Co Lid,Hunan Valin Gnup,Xiangan 411101
  • Received:2007-12-03 Online:2008-06-01 Published:2022-12-22

湘钢低碳贝氏体钢XDB685的研制

夏政海, 曹 波,   曹志强   

  1. 湖南华菱湘潭钢铁有限公司湘钢科技开发中心,湘潭411101
  • 作者简介:夏政海(1966-),男,工程师,1988年东北大学毕业,特殊钢新产品研发。

Abstract: A low carbon Bainitic steel XDB685[≤0.09C,1.20~1.60Mn,0.015~0.055Nb,0.008~0.030Ti, 0.2~0.6(Cr+N+Mo+B)] has devebped by using TMCP(Themomechanical Controlecd Pnsess)- RPC(Rdlaxed Pncess Contal)"-T(Tempering)technology. Test esulls showed thet the yidld strengh of40~60 mm steel plate was ≥600 MPa,the tensile strengih was ≥700 MPa, the impact energy at -40℃ was about 200 J,and the steel plate had excellent weldability.

摘要: 采用TMCP(Thermomechanical controlled Process)-RPC(Relaxed Process Control)-T(Tempering)工艺研制了低碳贝氏体钢XDB685[%:≤0.09C、1.20~1.60Mn、0.015~0.055Nb、0.008~0.030Ti、0.2~0.6(Cr+Ni+ Mo+B)]。检验结果表明,40~60 mm钢板的屈服强度≥600 MPa,抗拉强度≥700 MPa,-40℃冲击功约为200 J,并具有良好的焊接性能。