ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2008, Vol. 29 ›› Issue (4): 25-27.

Previous Articles     Next Articles

Experiment of Deoxidation and Desulphurization for X120 Pipeline Steel Melting by Vacuum Induction Furnace

Yao   Chunfa1, Li   Taiquan2, Wang   Min2, Li   Guangying1   

  1. 1 Central Iron and Steel Research Institute,Beijing 100081;
    2 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2008-02-11 Online:2008-08-01 Published:2022-12-23

真空感应炉冶炼X120管线钢脱氧和脱硫试验

姚春发1,李太全2, 王 敏2, 李光瀛   

  1. 1钢铁研究总院结构材料研究所,北京100081;
    2北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:姚春发(1964-),男,工程师,北京化工学院毕业,真空感应炉冶炼工艺研究。

Abstract:  The   test    of   deoxidation    and    desulphurization    of   X120   pipeline    steel-0.03~0.04C,1.98~2.05Mn,≤   0.9(Cr+Mo+Nb+V+Ti)has  been   caried   out  by   150  kg   and   50  kg  vacuum   induction   furnace  with  magnesium   oxide crucible. Results showed that with controlling carbon-oxygen reaction using carbon for deoxidiza tion and controlling melting  temperature  to  avoid  furnace  lining  decomposition,  the  oxygen  content  in  steel  was  ≤20×10-6 and  with  CgO-BaO-CaF2 fining  slag  the  sulphur  content  in  steel  was≤0.002%.It  was  found  by  scanning  electron  microscope  that  there  was  ≤5  μm MgO inclusions in  steel which originated from crucible.

Key words:  , X120 Pipeline Steel,Vacuum Induction Furnace,Deoxidation,Desulphurization

摘要: 在150 kg和50 kg氧化镁坩埚真空感应炉上进行X120管线钢(%:0.03~0.04C、1.98~2.05Mn、≤0.9(Cr+Mo+Nb+V+Ti)的脱氧和脱硫试验。结果表明,通过控制碳氧反应用碳脱氧和控制冶炼温度避免炉衬分解,可使钢中氧含量≤20×10-6;在碳脱氧条件下,采用CaO-BaO-CaF2系精炼渣,可使钢中硫含量≤0.002%。通过扫描电镜观察发现,钢中存在来源于坩埚的≤5μmMgo夹杂。