Xing Wei, Ni Hongwei, Shen Qiaozhen, Zhang Hua, He Huanyu. Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model[J]. Special Steel, 2007, 28(4): 13-15.
1 张鉴.炉外精炼的理论与实践.北京:冶金工业出版社,1991
2 朱苗勇,萧泽强.钢的精炼过程数学物理模拟.北京;冶金工业出版社,1998
3 李碧霞,高文芳,颜正国.大包底吹氩水模实验研究.炼钢,2001, 17(4):44
4 Jonsson L. Modeling of Fluid Flow Conditions Amund the Slag/Metal Interface in a Gas-stirred Ladle. ISIJ International,1996,36(9):1127
5 Pan Y,Bjrkman B.Numerical Analysis on the Similarity Between Steel Ladles and Hot-water Models Regarding Natural Convection Phenomena. ISIJ International,2002,42(1):53
6 Han JW,Heo S H.Transient Fluid Flow Phenomena in a Gas Stirred Liquid Bath with Top Oil Layer-Approach Numerical Simulation and Water Model Experiments. ISIJ Intemational,2001,41(10):1165
7 谢蕴国.小型钢包吹氩搅拌混合现象研究.昆明工学院学报,1989,14(1);41
8 张俊锡,罗建军,张际辉.第三炼钢厂90吨钢包吹氩水模型试验研究.首钢科技,1996(16):12