Analysis on Finite Element Simulation for Effect of Roll Diameter Ratio on Rolled Strip Flatness
Zhao Baolu1, Lu Jiansheng1, Song Peng1, Zhang Defeng2, Song Qunling2, Ning Deyu3 , Yang Hao3
1 Faculty of Materials and Metallurgical Engineering, Kunming University of Science and Technology, Kunming 650093;
2 Kunming Metallurgical College, Kunming 650033 ;
3 Kunming Iron and Steel Group Co Ltd, Kunming 650302
Zhao Baolu, Lu Jiansheng, Song Peng, Zhang Defeng, Song Qunling, Ning Deyu, Yang Hao . Analysis on Finite Element Simulation for Effect of Roll Diameter Ratio on Rolled Strip Flatness[J]. Special Steel, 2007, 28(4): 27-29.