Structure Evolution of 0.75C Eutectoid Carbon Steel during Reduction Deformation

Zhang Shulan, Sun Xinjun , Dong Han   

  1. Institute of Structure Materials,Central Iron and Steel Research Institute,Beijing 100081
  • Received:2006-06-30 Online:2007-01-01 Published:2023-01-13

0.75C共析钢压缩变形时的组织演变

张淑兰,  孙新军,  董 瀚   

  1. 钢铁研究总院结构材料研究所,北京100081
  • 作者简介:张淑兰(1978-),女,博士研究生,2001年华北工学院毕业,从事结构材料研究。

Abstract: The structure evolution of pearlite and overcooling austenite of 0.75C eutectoid carbon steel during com- pression has been studied by Gleeble 2000 and 1500 thermal simulation machines.The test results showed that as sample heated with 10 ℃/s to700 ℃ for 3 min than carried out 60% reduction,the lamellar pearlite in steel broke up and frac- tured; and as sample heated to 1150 ℃ for 1 min for austenization than cooled with 20 ℃/8 to 700 ℃ and reduced by 60%,the partial overcooling austenite in steel transformed to fine lamellar pearlite under effect of deformation.

Key words: Eutectoid Steel, Austenite, , Pearlite, , Deformation

摘要: 通过Gleeble 2000和1500热模拟试验机,研究了0.75C共析钢珠光体和过冷奥氏体在压缩变形过程 中的组织演变。试验结果表明,试样以10℃/s加热至700 ℃ 3 min进行60%压缩变形,钢中珠光体片层发生断裂、 破碎;试样加热至1150℃1 min奥氏体化后以20℃/s冷却至700 ℃,压缩变形60%,在变形作用下,钢中部分过冷奥氏体转变成细片层珠光体。