Behavour of Non-metallic Inclusions in Liquid Alloy Steel under High Basicity High A12O3 Slag

Chen Bin, Jiang Min and Wang Xinhua   

  1. Metallurgical and Ecological Engineering School, University of Science and Technology, Beijing 100083
  • Online:2008-04-01 Published:2023-01-16

高碱度高AI2O3炉渣下合金钢液中非金属夹杂物的行为

陈斌  姜敏  王新华   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:陈斌(1980-),男,博士研究生,控制钢中夹杂物,提高钢 材的抗疲劳性能

Abstract:

 Ingredient and morphology of structure of inclusions in liquid alloy steel (0. 42C, 1. 14Cr, 0. 23Mo) under high basicity slag 43 -47CaO - 5 - 10SiO2 - 46 -54A1203 have been studied by silicon molybdenum electric resistance furnace with MgO crucible. It was obtained that after reaction with high basicity high A12O3 slag for 90 min, most of inclusions formed in liquid steel were calcium-magnesium-aluminum silicate inclusions which were easily removed from liquid steel, and the inclusions remained in steel were global particles being available to improve the fatigue resistance of steel products. It was available to fonn calcium-magnesium-aluminum silicate inclusions as the basicity of slag was 9.

Key words:  , Alloy Steel, High Basicity High Al2O3 Slag, Inclusions

摘要: 通过MgO地垠硅铝电阻炉研究了(% ):43~47CaO-5 ~ 10SiO2-46~54A12O3高碱度炉渣下合金钢 液(%:0. 42C、1. 14Cr、0. 23Mo)中夹杂物的成分和组织形貌。结果得出,高碱度高A12O3炉渣和钢液反应90 min 后,钢中主要生成低熔点钙镁铝硅酸盐夹杂,该夹杂大部分上浮去除,留在钢中的为球形夹杂,有利于提高钢材的 抗疲劳性能。当炉渣碱度约为9时,有利于生成钙镁铝硅酸盐夹杂。