Evolution of Structure and Texture Orientation of 50W600 Cold Rolled Non-Orientation Electrical Steel during Annealing

Zhang Hongjie,Jin Zili and Wang Yufeng   

  1. Faculty of Materials Science and Metallurgy,Inner Mongolia University of Science and Technology,Baotou 014010
  • Online:2008-04-01 Published:2023-01-17

50W600冷轧无取向电工钢退火过程组织和织构取向的演变

张红杰  金自力 王玉峰   

  1. 内蒙古科技大学材料与冶金学院,包头014010
  • 作者简介:张红杰(1980-),女,硕士研究生,沈阳理工大学毕业,先进 材料组织、织构和性能研究。

Abstract: Structure  and  texture  orientation  of  50W600  cold  rolled  non-orientation  electrical  steel(0.003~0.008C,0.3Si)during  annealing  at  700~760  ℃  for  3~360  s,water  cooling  have  been  studied  by  metallography  and  electron  back-scattering  spectrum  difraction  analysis.Results  showed  that  incrensing  annealing  temperature  the  rate  of recrystaliza-tion and grain size increased; during annealing at 740 ℃,as annealing time increased from  10 s to 360 s,the rate of recrys-tallization increased from 22.5% to  100% and average grain size increased from 3.08  μm to  17.17 μm,and the density of  recrystallization texture at α- fibre decreased,as annealing for  15 s the density of {001}〈110〉,{112}〈110〉,{111}〈110〉 and {110}〈110〉was abot 1.5 and the density of {111}〈011〉 and {111}〈112〉at γ-fibre was steadily about 0.25.

摘要: 通过金相和电子背散射衍射法(EBSD)研究50W600冷轧无取向电工钢(0.003%~0.008%C、0.3% Si)在700~760℃3~360s退火水冷时的组织和织构取向演变。结果表明,随退火温度的提高,钢的再结晶率和 晶粒尺寸增大,740℃退火时,当保温时间由10s增加至360s,再结晶率由22.5%提高到100%,平均晶粒尺寸由 3.08μm增大至17.17μm。同时再结晶织构α线的取向密度下降,在15s时[001}<110〉、{1121<110〉、{1111 <110〉、{110〈110〉的取向密度均为1.5左右,y线上{111}<011〉和{111}〈112〉的取向密度稳定在0.25左右。