Nanocrystallization Technology and Corrosion Resistance of#br# Stainless Steel#br#

Zhen Zhijun and Gao Yan   

  1. School of Mechanical Engineering,South China University of Technology,Guangzhou 510641
  • Online:2008-04-01 Published:2023-01-19

不锈钢的纳米化工艺及其耐腐蚀性

郑志军  高  岩   

  1. 华南理工大学机械工程学院,广州510641
  • 作者简介:郑志军(1974-),男,讲师,2003年华南理工大学毕业,金属 纳米材料的制备和性能研究

Abstract: The surface nanocrystallization technology of stainless steel such as surface mechanical attrition treatment,  shot peering,cross shear rolling and laser surface melting and the bulk nanostructured technology such as mechanical alloy  method,inert  gas  condensation  in-situ  compression,electrochemical  deposition,crystallized  from  amorphous  solid  and  se- vere plastic deformation method is presented. The corrosion resistance of nanocrystallined stainless steel is affected directly by  nanocrystalline  structure  and  the  features  including  uniform  structure,free-dislocation  and  intemal  stress  are  precondi-  tions to get excellent corrosion resistance.

Key words: Stainless Steel,Nanocrystallization Technology,Corrosion resistance

摘要: 叙述了不锈钢表面纳米化技术-表面机械研磨处理,喷丸法,异步轧制法和激光表面融熔法和不锈钢 块体纳米化技术-机械合金法,惰性气体凝聚原位加压法,电化学沉积法,非晶晶化法和大塑性变形法。纳米化不锈 钢的耐蚀性能直接受到纳米晶结构的影响,结构均匀,无位错,无应力是获得优异耐蚀性的前提。