ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (3): 35-37.

Previous Articles     Next Articles

Effect of Cooling Rate on Structure Evolution of Hot Deformed Ferrite-Bainite Micro Alloying Steel

Guan  Li,Liu  Yazheng,Zhou  Leyu , Song  Renbo   

  1. School of Materials Science and Engineering, University of Science and Technology, Beijing 100083
  • Received:2006-12-22 Online:2007-05-01 Published:2023-02-03

热变形后冷却速度对铁素体-贝氏体微合金钢组织演变的影响

管丽,刘雅政,周乐育,宋仁伯   

  1. 北京科技大学材料科学与工程学院 ,北京 100083
  • 作者简介:管丽(1982-),女,硕士研究生,汽车车轮用钢的研究。
  • 基金资助:
    中信-CBMM铌钢研究与开发基金资助项目(编号: 2006RMJS-D017)

Abstract: Ferrite-bainite(F+B)microalloying  steel0.06C-1.08Si- 1.64Mn-0.30Mo-0.039Nb-0.01Ti  has   been  developed;  continuous  cooling  transformation(CCT)diagram  of  50%  deformed  test  steel  at  900  ℃  and  with  cooling  rate 0.5~40  ℃/s  was  obtained  by  Cleeble-1500  thermal  simulator,and  phase  transformation  structure  of  deformed  austenite was analyzed. Results  showed that the CCT diagram was composed of polygonal ferrite transformation region and bainite transformation region which were  divided by metastable  austenite region;  as  cooling rate was≤2  ℃/s,polygonal  ferrite  occurred  in  steel  and  as the  cooling rate was ≥5  ℃/s,main  structure  in  steel  consisted  of granular bainite  and  lath bainite.

Key words: Ferrite-Bainite ,  , Steel, Hot ,  , Deformation, Cooling ,  , Rate, Structure ,  , Evolution, CCT ,  , Diagram

摘要: 开发了0.06C-1.08Si-1.64Mn-0.30Mo-0.039Nb-0.01Ti铁素体-贝氏体微合金化(F+B)钢;用Gleeble.1500热模拟机测定了该实验钢在900℃变形50%后0.5~40℃/s冷却速度下的连续冷却转变曲线(CCT),并分析了形变奥氏体的相变组织。结果表明,该钢的CCT曲线分为多边形铁素体转变区和贝氏体转变区两大部分,中间被奥氏体亚稳区隔开;当冷速≤2℃/s时,钢中出现多边形铁索体,当冷速≥5℃/s时,组织主要为粒状贝氏体和板条贝氏体。