ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (3): 50-52.

Previous Articles     Next Articles

Present  Status  and  Development  Trend  of  Stainless  Steel  in  China

Cheng Penghui,He Dongfeng ,Tian Naiyuan   

  1. University of Science and Technology,Beijing 100083
  • Received:2006-11-01 Online:2007-05-01 Published:2023-02-03

我国不锈钢发展现状及展望

程鹏辉,贺东风,田乃媛   

  1. 北京科技大学,北京100083
  • 作者简介:程鹏辉(1980-),男,北京科技大学毕业,硕士研究生,北京科技大学冶金工程与战略研究中心,冶金流程工程研究及钢 铁行业资讯。

Abstract: The  amount  of  annual  apparent  consumption  of  stainless  steel  in  China  in  2005  was  up  to5220000  t,  being  6  times  the  amount  of  annual  apparent  consumption  in  1998,at  the  some  time  the  amount  of  annual  output  of  stainless steel  in  China  increased  to  3160000  t  in  2005  from  220000  t  in  1998  and  the  shortage  was  compensated  mainly  by  input.  According  to  incomplete  statistic,up  to  the  end  of  2006,the  production  capacity  of  hot  rolled  stainless  steel  in  China  shall be  up  to10000000  t  per  year  and  that  of  cold  rolled  stainless  steel  shall  be  more  than  5000000  t  per  year.  Relative  issues in  development  of  stainless  steel  are  discussed  in  this  article  and  it  is  predicted  that  stainless  steel  requirement  amount  of stainless   steel   in   China   in   2010   shall   be 8410000~10500000 t,in   which   300   series   austenite   steels   make   up   50%~ 60%,400 series    ferrite    stainless    steels   make   up    30%~35%,anothers    including    200    series   make   up5%~10%.

Key words:  , Stainless Steel, Production, Consumption, Prediction

摘要: 2005年我国不锈钢的表观消费量达522万t,是1998年的6倍;同时我国不锈钢的年产量也从1908年的22万t增加至2005年的316万t,主要通过进口弥补不足部分。据不完全统计,到2006年底,我国热轧不锈钢产能将达到1000万t/a,冷轧不锈钢产能将超过500万t/a。文中讨论了不锈钢发展过程的有关问题,并预测我国2010年不锈钢需求量为841~1 050万t,其中300系列奥氏体不锈钢占50%~60%,400系列铁索体不锈钢占30%~35%,其他(包括200系列)占5%~10%。