Numerical Simulation of Flow Field of Molten Steel in Tundish for Slab Concasting and Operation Optimization

Jia Lingfeng , Sun Yuping , Yue Kexiang   

  1. Metallurgy and Resources School, Anhui University of Technology, Maanshan 243002
  • Received:2005-11-06 Online:2006-04-01 Published:2023-03-02

板坯连铸中间包钢液流场的数值模拟和操作优化

贾凌锋,孙于萍,乐可襄   

  1. 安徽工业大学冶金与资源学院,马鞍山 243002
  • 作者简介:贾凌锋(1981-),男,在读硕士研究生,从事冶金、热能、冶金过程仿真节能技术研究。

Abstract: Taking tundish for No4 Slab concaster at Nol steel plant, Jinan Steel, computer numerical simulation for difierent weir and dam design scheme was carried out to optimize design of weir and dam in tundish by using turbulent flowage math model. Results showed that for tundish with top dimensions 3500 mm x 800 mm, bottom dimensions 3200 mm x 650 mm and molten steel depth in tundish 800 mm, molten steel had better flowage condition as weir height 550 mm, dam hei^it 350 mm, distance between weir and nozzle entrance 800 mm and relative distance between weir and dam 400 mm, it was available inclusions floating off.

Key words: Slab Concasting, Tundish, Steel Flow Field, Numerical Simulation

摘要: 以济钢第一炼钢厂4#板坯连铸中间包为原型,应用湍流流动数学模型对不同堰坝设计方案进行计算机数值模拟,优化中间包的堰坝设计。结果表明,对上口面积3500 mm × 800 mm、底部面积3200 mm × 650 mm的中间包,包内钢水深度为800 mm时,当挡堰高550 mm,挡坝高350 mm,挡堰与水口入口处距离800mm,挡堰与挡坝相对距离400 mm时,钢液具有较好的流动方式,有利于夹杂物上浮。

关键词: 板坯连铸, 中间包, 钢水流场, 数值模拟