Effect of Modifying Agent on Melting Point and Desulphurizing Capacity of LATS Refining Slag

Li Bo   

  1. Steelmaking Shop,Stainless Steel Branch,Baosteel Group,Shanghai 200431
  • Received:2006-12-05 Online:2007-04-01 Published:2023-03-10

调质剂对 LATS 精炼渣熔点与脱硫能力的影响

李  波   

  1. 宝钢股份不锈钢分公司炼钢厂,上海200431

  • 作者简介:李 波(1972-),男,工程师,博士研究生,从事精炼技术研究与开发。

Abstract: The CaO-CaF2, CaO-B2O3and Li2O were respectively used as modifying agent adding to ladle slag to decrease slag adhesion of LATS-OB refining immersion cover and increase service life of cover. Test results of melting point of slag measured by hemisphere method showed that using, CaO:CaF2=1~2,CaO:B2O3=1~2 or Li2O as modifying agent could remarkably decrease melting point of ladle slag. And metal-slag equilibrium test indicated that the sulphur content in steel further decreased by ladle slag added modifying agent.

摘要: 为减少LATS-OB精炼浸渍罩粘渣及提高浸渍罩寿命,分别用CaO-CaF2、CaO-B2O3及Li2O作为钢包渣的调质剂进行调质实验。熔渣半球点法的熔点测试结果表明,采用CaO/CaF2=1或2,CaO/B2O3=1或2和Li2O作调质剂能显著降低钢包渣的熔点;渣-金平衡试验表明,调质后的钢包渣可使钢中的硫含量进一步降低。