Effect of Inner Cooling Apparatus -U Shape Pipe on Flow of Molten Steel in Slab Continuous Casting Mold

Jin Yanjuan ,Cui Xiaochao   

  1. School of Application Science, Taiyuan University of Science and Technology, Taiyuan 030024
  • Received:2006-01-09 Online:2006-05-08 Published:2023-03-10

内冷却器-U形管对板坯连铸结晶器内钢水流动的影响

晋艳娟,崔小朝   

  1. 太原科技大学应用科学学院,太原030024
  • 通讯作者: 崔小朝
  • 作者简介:晋艳娟(1979-),女,太原科技大学研究生,从事液态金属 流动多场耦合数值模拟研究。
  • 基金资助:
    国家自然科学资金资助项目(编号:50474013)

Abstract: A technology of inner-outer couple cooling of molten steel in mold for 1 240 mm x 200 mm slab concasting i, e, to set an inner cooling apparatus- U shape pipes has been advanced to enhance efficiency of heat transfer and improve flow of molten steel. The flow status of molten steel in the inner-outer couple cooling mold was simulated by using fluid dynamics software. It is found that the flow status of molten steel in mold is uniform by using inner U- shape cooling apparatus, which has effect of electromagnetic trig to be favourable to inclusion in steel floating up.

Key words: Inner Cooling Apparatus, Slab Concasting, Molten Steel, How, Simulation

摘要: 针对1 240 mm×200 mm板坯连铸提出了一种钢水内外复合冷却技术,即在“结晶器内设置内冷却器-U形管”,起到提高传热效率和改善钢液流动之目的。运用流体力学分析软件,就内外复合冷却结晶器内钢水的流动状态进行了数值模拟,发现内冷却器可以使结晶器内钢水的流动状态均匀,部分起到电磁制动之功效,有利于钢液中的夹杂物上浮。

关键词: 内冷却器, 板坯连铸, 钢水, 流动, 模拟