Influence of Solution Temperature on Structure and Properties of Super Duplex Stainless Steel 00Cr25Ni7Mo4N

Wu Zhongzhong1.2, Song Zhigang2, Zheng, Wenjie2, Chen Bin2, Lu Jiansheng1   

  1. 1 Faculty of Materials and Metallurgical Engineering, Kunming University of Science and Technology, Kunming 650093;
    2 Center Iron and Steel Institute, Beijing 100081
  • Received:2006-01-26 Online:2006-08-01 Published:2023-03-17

固溶温度对超级双相不锈钢00Cr25Ni7Mo4N 组织和性能的影响

吴忠忠1.2,宋志刚2,郑文杰2,陈  斌2,陆建生1   

  1. 1昆明理工大学材料与冶金工程学院,昆明650093;2钢铁研究总院结构材料研究所,北京100081
  • 作者简介:吴忠忠(1978-),男,材料学专业,硕士研究生,从事不锈钢研究。

Abstract: The phase composition, impact energy Akv and hardness HRC value of duplex stainless steel 00Cr25Ni7Mo4N solution treated at 900~1300 ℃ have been studied and examined. The results showed that 16.97%~ 3.22% a- phase precipitated in duplex stainless steel during solution treatment at 900~1020 ℃ led to the impact energy Agy value of steel decreasing to 3~44 J from 224~280 Jwhile steel treated at 1040~1250 ℃. The hot work temperature of the duplex stainless steel should be higher than 1040 ℃ and its optimum solution treatment temperature is 1040~1100 ℃.

摘要: 试验和测试了900-1 300℃固溶处理时双相不锈钢00Cr25Ni7Mo4N的相组成、冲击能AKV和硬度(HRC)值。试验结果表明,在900-1 020℃固溶处理时,双相不锈钢中有16.97%-3.22%σ相析出,使钢的冲击能Akv值从1 040-1 250℃处理的224~280 J降至3~44 J。该双相不锈钢的热加工温度应大于1 040℃,其最佳固溶处理温度为1 040~1 100℃。