An Analysis on Nano-Scaled Precipitates in Microalloyed High Strength Steels

Wu Huajie, Fu Jie, Liu Yangchun   

  1. School of Metallurgical and Ecological Engineering, University of Science and Technology,Beijing 100083
  • Received:2006-01-17 Online:2006-08-01 Published:2023-03-17

微合金高强度钢纳米级析出相的分析

吴华杰, 傅杰,刘阳春   

  1. 北京科技大学冶金与生态工程学院,北京100083
  • 作者简介:吴华杰(1978-),男,博士研究生,钢铁冶金工艺和金属材料研究。
  • 基金资助:
    国家自然科学基金资助项目(50334010)

Abstract: The precipitated phase composition, mass percent and particle size distribution in microalloyed high strength steels 70A(0.05C,1.90Mn,0.01V,0. 13Ti,0.06Nb) and B2C (0.06C,2.34Mn,0.03V,0.03Ti,0.04Nb,0.0067 B) have been studied by chemical phase analysis and small-angle X- ray scattering method. It was found that there were nano-scale M2C and M2C6 carbide in large amounts in microalloyed steels:the mass percent of M3C + M2Ccarbide in diameter less than 36 nm in steel 70A was 0.0664% and the mass percent of MC carbide in same diameter was 0.0371%; and that of M3C + M23C6carbide in diameter less than 36 nm in steel B2C was 0. 1341% while that of the MC in same diameter was 0.0084%.

Key words:  , Microalloyed Steel,Nano-Scaled Carbide,Phase Analysis

摘要: 用化学相分析加X-射线小角散射法对微合金高强度钢70A(%:0.05C,1.90Mn,0.01V,0.13Ti, 0.06Nb)和B2C(%:0.06C,2.34Mn,0.03V,0.03Ti,0.04Nb,0.0067B)的析出相结构、质量分数和粒度分布进行了研究。结果发现,微合金化钢亦存在大量纳米级M3C和M23C6碳化物,70A钢中<36 nm的M3C+M23C6碳化物质量分数为0.0664%,同尺寸的MC碳化物为0.0371%;B2C钢中<36 nm的M3C+M23C6碳化物的质量分数为0.134 1%,同尺寸的MC为0.008 4%。

关键词: 微合金化钢,纳米级碳化物, 相分析