Special Steel ›› 2006, Vol. 27 ›› Issue (4): 31-33.

Previous Articles     Next Articles

Effect of Normalizing Temperature on Structure and Magnetic Properties of Annealed Non-Oriented Electric Steel

Jian Ruixiong 1,2, Zhang Wenkang2,1, Du Zhengnin1, Mao Weimin1, Wang Yide2   

  1. 1 School of Materials Science and Engineering, University of Science and Technology,Beijing 100083;
    2 Technical Center, Taiyuan Iron and Steel(Group)Co Lid, Taiyuan 030003
  • Received:2006-02-25 Online:2006-08-01 Published:2023-03-17

热轧板常化温度对冷轧无取向电工钢退火组织和磁性能的影响

菅瑞雄1,2, 张文康2,1, 杜振民1, 毛卫民1,王一德2   

  1. 1北京科技大学材料科学和工程学院,北京100083;
    2太原钢铁(集团)有限公司技术中心,太原030003
  • 作者简介:菅瑞雄(1973-),男,硕士研究生,1997年西安建筑科技大学毕业,冷轧无取向电工钢的研发。

Abstract: The effect of 2.5 mm hot rolled plate of electric steel(≤0.005%C-2.5%~2.8%Si)normalizing at 850 ~1100℃ on structure and magnetic properties of 0.5 mm cold rolled sheet annealed at 880 ℃+ 950 ℃ has been studied.The results showed that with increasing normalizing temperature of hot rolled plate,the recrystallized grain size of annealed cold rolled sheet increased,iron loss reduced and magnetic induction monotonically increased; as normalizing temperature was more than 1000 ℃,with solid solution second phases then precipitated dispersed in annealed cold rolled sheet,the grain fined and iron loss increased. The optimum normalizing temperature of hot rolled plate is 1000 ℃.

摘要: 研究了≤0.005%C-2.5%~2.8%Si的2.5 mm热轧电工钢板在850~1 100℃常化对0.5 mm冷轧板880℃+950℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感呈单调递增趋势;热轧板常化温度超过1 000℃,因第2相固溶而后弥散析出,退火冷轧晶粒细化,铁损增加,因此该钢热轧板最佳常化温度为1 000℃。

关键词: 无取向, 电工钢, 热轧板常化, 组织, 磁性能