Nitrogen-Bearing Duplex Stainless Steel and Its Metallurgical Technology

Li   Xuefeng1, Li   Zhengbang2   

  1. 1 Quality Department,Taiyuan lron and Steel(Group)Co Lid,Taiyuan 030003;
    2 Central Iron and Steel Research Institute,Beijing 100081)
  • Received:2006-03-16 Online:2006-08-01 Published:2023-03-17

含氮双相不锈钢及其冶金工艺

李学锋1,李正邦2   

  1. 1太原钢铁(集团)有限公司品质部,太原030003;
    2钢铁研究总院,北京100081
  • 作者简介:李学锋(1964),男,教授级高工,从事不锈钢工艺、技术、 品种和质量的研究和管理。

Abstract: As compared with austenite stainless steel, the ferrite-austenite duplex stainless steel has higher mechanical properties, excellent stress and pitting corrosion, and lower cost due to lower Ni content, especially improve weldability of steel due to lower carbon content and higher nitrogen content in steel. Higher nitrogen content in duplex stainless steel has two favourable factors: depressing formation of δ ferrite and increasing pitting resistance equivalent. The 4 kinds of nitrogen bearing duplex stainless steel grades, and designation and chemical compositions of conventional duplex stainless steel;5 kinds of metallurgical processes; production of duplex stainless steel at Taiyuan Steel, thermomechanical processing for duplex stainless steel and trend of research and development of duplex stainless steel are presented in this article.

摘要: 铁素体-奥氏体双相不锈钢比奥氏体不锈钢有较高的机械性能、优良的耐应力腐蚀和点腐蚀性能以及较低的价格(Ni含量低),特别是通过降低钢中的碳含量和增加氮含量而改善了钢的可焊性。双相钢中含较高的氮含量有两个有利的因素:抑制δ-铁素体的形成和提高抗点蚀当量。介绍了4种不同类型的含氮双相不锈钢和常用双相不锈钢的牌号和化学成分、双相不锈钢5种冶金工艺、太钢双相不锈钢的生产、高氮双相不锈钢的形变热处理以及双相不锈钢的研究和发展趋势。

关键词: 含氮, 双相不锈钢 , 冶金工艺