Research and Application of Ferrite Rolling at Home and Abroad

Xu Guang1 , Xu Chushao2 , Zhao Jiarong1   

  1. 1. Wuhan University of Science and Technology, Wuhan 430081;
    2. School of Materials and Metallurgy, Chongqing University, Chongqing 400044;
  • Received:2005-03-04 Online:2005-10-01 Published:2023-03-31

国内外铁素体轧制的研究和应用

徐光1,徐楚韶2,赵嘉蓉1   

  1. 1. 武汉科技大学,武汉 430081;
    2. 重庆大学材料科学与工程学院,重庆 400044;
  • 作者简介:徐光(1961-),男,教授,1982年北京科技大学毕业,1987年武汉科技大学研究生毕业。从事金属加工工艺和组织性能研究。

Abstract: Ferrite rolling-warm rolling for <1.2 mm extra-thin hot rolling strip can save energy and decrease production cost. Current quick development of dun slab continuous casting and rolling technology contributes a good condition to develop and apply the ferrite rolling. Hie low carbon steel thin sheet and microalloying steel thin sheet have been produced by ferrite-warm rolling process. The research status of flow stress, recrystallization, microstructure and properties of ferrite rolled products, and application situation of ferrite rolling are summarteed in this paper.

Key words: Thin Strip, Ferrite Rolling, Flow Stress, Recrystallization, Structure and Properties

摘要: 超薄热轧带钢(<1.2mm)的铁素体轧制(低温轧制)能显著节约能源和降低生产成本。当前迅速发展的薄板坯连铸连轧技术为铁素体轧制的发展与应用创造了良好的条件。已采用铁素体温轧工艺的钢板为低碳钢薄板和微合金化钢薄板。总结了铁素体轧制时流动应力,再结晶,轧后产品组织和性能的研究现状和铁素体轧制的应用情况。

关键词: 薄带, 铁素体轧制, 流动应力, 再结晶, 组织和性能