Effect of BaO and Li2O on Melting Point and Viscosity of CaO-Based Refining Fluxes for Desulphuration

Li Guirong,Zhu Zhenxue,Dai Qixun and Wang Hongming   

  1. School of Materials Science and Engineering, Jiangsu University, Zhenjiang 212013

  • Received:2005-01-19 Online:2005-08-01 Published:2023-04-08

BaO 和 Li2O 对 CaO 基脱硫精炼渣熔点和粘度的影响

李桂荣, 祝贞学,戴起勋, 王宏明   

  1. 江苏大学材料科学与工程学院,镇江212013
  • 作者简介:李桂荣(1976-),女,博士研究生,从事炼钢工艺研究。
  • 基金资助:
    国家自然科学基金项目(50474037),
    江苏省高校 自然科学研究项目(04BJK430022)

Abstract: The melting point and viscosity of refining fluxes for desulphuration have been studied of which CaO (balance)-SiO(22.4%)-Al2O2(11.6%)-CaF(10%) refining slag was as basic flux, when the ratio of (CaO+RxO)/SiO2 was fixed at 2.5(where RxO- BaO or Li2O), the BaO or Li2O added and replaced equivalent CaO content in flux. The results showed that the melting point and viscosity of fuxes decreased by added BaO or Li₂O in CaO basic slag effectively to improve the dynamics condition of metal- slag reaction. With 15% BaO or 15%Li₂O,the melting point of flux was 1267 ℃  or 1185 ℃ which were far lower than that of flux free additions- 1326 ℃,and the viscosity of flux at 1475 ℃ was 0.98 Pa · s or 0.51 Pa · s which were also far lower than that of flux free additions- 1.79 Pa · s to make the fluxes had excellent flu-  idity and melting capacity.

Key words:  , CaO Based Fux,BaO,Li?O,Melting Point,Viscosity

摘要: 以CaO(bal)-SiO2(22.4%)-Al2O2(11.6%)-CaF2(10%)精炼渣作为基础渣系,用BaO、Li2O替代其中等量的CaO含量,固定(CaO+RxO)/SiO2=2.5(RxO代表BaO或者Li2O),对该脱硫精炼渣系的熔点和粘度进行了研究。结果显示在传统的CaO基熔渣中加入BaO、Li2O可以降低渣系的熔点和粘度,有效地改善了渣钢反应的动力学条件。当(BaO,Li2O)=15%时,熔渣的熔点分别为1267℃和1185℃,远低于不加添加剂时的熔点1326℃,当温度为1475℃时,熔渣粘度分别为0.98Pa·s和0.51Pa·s,远小于不加添加剂时的粘度1.79Pa·s,使渣系具有良好的流动性和熔化性能。

关键词: CaO 基熔渣, BaO, , Li2O, , 熔点, 粘度