ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (6): 5-7.

Previous Articles     Next Articles

A Study on Distribution Characteristics of Electromagnetic Field in Concasting Mould for Round Bloom

Guo Shangxing, Wang Jianjun, Zhou Li, Li Weiguo , Shi Xiaofang,Sun Wei ,Wang Kaizhong   

  1. School of Metallurgy and Resources, Anhui University of Technology, Maanshan 243002
    Maanshan Iron and Steel Co Ltd, Maanshan 243000
  • Received:2005-05-24 Online:2005-11-08 Published:2023-04-11

大圆坯连铸结晶器内电磁场分布特性的实验研究

郭上型,王建军,周俐,李卫国,施晓芳,孙维,汪开忠   

  1. 安徽工业大学冶金和资源学院,马鞍山243002
    马鞍山钢铁股份有限公司,马鞍山243000
  • 基金资助:
    国家高技术研究发展专项经费资助项目 (2003AA331160)

Abstract: In condition of commercial production at Maanshan Steel, with electric current parameter within limits 400 ~ 510 A and 2.0 ~ 2.5 Hz, the distribution characteristics of magnetic induction intensity in concasting mould with M-EMS for 8380 mm round bloom has been measured by using Gauss-meter. Hie results showed that the curve of magnetic induction intensity along vertical direction of mould center had a peak shape and the maximum value was at M-EMS stirrer center and a distance 530 mm from top of mould; and it increased gradually from center to edge at mould horizontal section. The magnetic induction intensity at meniscus was about 10% of that maximum value at mould middle section. Hie analysis shows that in the present production conditions at Maanshan Steel the stirring intensity with using electric current parameter 400 A/2.5 Hz is not enough.

Key words:  , Round Bloom, Concasting, Mould, Electromagnetic Stirring, Magnetic Induction Intensity

摘要: 在马钢工业生产条件下,用高斯计空载测量Φ380 mm圆坯连铸结晶器内在电流参数400~510A、2.0~2.5 Hz的范围内磁感应强度的分布特性。结果表明,结晶器中心垂直方向磁感应强度变化曲线呈波峰状,在离结晶器上口约530 mm的电磁搅拌器中心处有最大值;在结晶器水平截面上磁感应强度沿截面中心至边缘逐渐增大。钢液弯月面处的磁感应强度是结晶器中心最大值的10%左右。马钢在现有生产条件下采用400 A/2.5 Hz的电流参数,相应电磁搅拌强度明显偏低。

关键词: 圆坯, 连铸, 结晶器, 电磁搅拌, 磁感应强度