Abstract: The large-volume are fumace and continuous caster for alloy steels were built and imported at domestic main special steel works during end of the nineties of 20th century thus to bush the development of continuous casting technology for special steel in China forward. The casting billet size of alloy steel was between 130 mmx130 mm and 350 mm×470 mm and alloy steel slab size was between 1030 mm x160 mm and 1900 mm×300 mm. The continuous casting production in percent of domestic special steel inereased from 21.7% in 1998 to 61. 17% in 2003. According to the key technology and advance of continuous casting at overseas' special steel producer, and based the analysis on production equipment, flow sheet, output of continuous casting billet and quality status of main continuous casting products in china in recent years,the development and research work for special steel continuous casting technology in China are put forward in this paper.
摘要: 20世纪90年代末,国内各主要特殊钢厂先后自建或引进大容量电弧炉和合金钢连铸机,从而推动了我国特殊钢连铸技术的发展。合金钢连铸方坯的规格为130mm×130 mm至350mm×470 mm,板坯为1030mm×160mm 至1900mm×300 mm。国内特殊钢连铸比由1998年的21.7%增加至2003年的61.17%。 根据国外特殊钢企业连铸关键技术和进展,以及对近几年我国特殊钢连铸生产装备、流程、生产量及主要产品质量现状的分析,提出了我国特殊钢连铸技术发展和研究的工作重点。
关键词: 特殊钢, 连铸技术, 发展
Gan Yong, Wang Zhongying. Present Status and Development of Continuous Casting Technology for Special Steel in China[J]. Special Steel, 2005, 26(3): 1-5.
干 勇, 王忠英. 国内特殊钢连铸生产技术的现状与发展[J]. 特殊钢, 2005, 26(3): 1-5.
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2005/V26/I3/1