A Study on Behavior of Hot Deformation of Ultra- Low Carbon Nb-V-Ti Microalloyed Steel

Zhou Jialin, Tang Li, Ren Yong,Li Lixin,Lii Xuebin, Yao Chengjun   

  1. College of Material and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081
    Wuhan Iron and Steel Group Company, Wuhan 430083
  • Received:2004-12-12 Online:2005-06-01 Published:2023-05-11

超低碳Nb-V-Ti微合金钢热变形行为的研究

周家林,唐力,任勇,李立新,吕学斌,姚成君   

  1. 武汉科技大学材料与冶金学院,武汉430081;
    武汉钢铁(集团)公司,武汉430083
  • 作者简介:周家林(1966-),男,硕士,讲师。主要从事材料成型过程 的数值模拟研究及成型工艺、设备方面的教学工作。

Abstract:  Based on the hot simulation test  the effect of deformation condition and microalloying element 0.018  0.056NB, 0.01 - 0.02V and 0.01 - 0.02Ti on behavior of hot deformation of 0.06 - 0.08C test steel has been analyzed. And based on the Sellas-Tartat equation, the mathematic models to calculate the stress- strain curves have been established, that are dynamic recover model σ(e)+ (σp+σo)[1-exp(-3.23ε/εs)]0.5, where σp- peak stress, σo- stress at onset of plasticstrain, ε- strain,εs-strain to onset of steady state by work hardening and recovering, and dynamic recrystallization model - σ=σ=σ(e)-(σpss){ 1- exp[-2.363(ε-εcc0.3425)2 , where σss-stress to onset of steady state by dynamic recrystallization, εc- strain for onset of dynamic recrystallization. The predicted results to rolling force by the models conform with that of measured value of 0.07C-0.018Nb test steel during commercial rolling.

摘要: 在热模拟实验的基础上,分析了变形条件及微合金元素Nb(0.018%~ 0.056%)、V(0.01%~ 0.02%)、Ti(0.01% ~0.02%)对0.06% ~0.08%C实验钢的热变形行为的影响。在Sellas-Tartat方程的基础上, 建立了应力-应变曲线数学模型:动态回复模型σ(e)+ (σp+σo)[1-exp(-3.23ε/εs)]0.5,式中:σp-峰值应 力,σo-初始应力,ε-变形应变,。σs-加工硬化与回复进入稳态的临界应变;动态再结晶模型σ=σ(e)-(σpss){ 1- exp[-2.363(ε-εcc0.3425)2}式中:σss-动态再结晶进入稳态时的应力, εc-心动态再结晶临界应变。利用该模 型对0.07%C ~ 0.018%Nb实验钢工业轧制时轧制压力进行了预测,其结果与实测值吻合良好。