ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (4): 52-53.

Previous Articles     Next Articles

Practice of Production of Spring Steel 65Mn by 100 t Converter-Ladle Furnace Refining concasting

Lu Ruiguo,Li Jingjun , Ruan Xibao   

  1. Xinyu Iron and Steel Co Ltd, Xinyu 338001
  • Received:2005-02-16 Online:2005-08-01 Published:2023-05-17

100 t转炉-钢包炉精炼-连铸生产65Mn 弹簧钢的工艺实践

吕瑞国,李京军,  阮细保   

  1. 新余钢铁有限责任公司,新余338001
  • 作者简介:吕瑞国(1966-),男,硕士,高级工程师,北京科技大学毕业。从事钢铁冶金工艺和新产品开发研究。

Abstract: The spring steel 65Mn was produced by 100 t top and bottom combined blown converter melting- ladle furnace refining- 6 strand 150 mm×150 mm billet concasting. The end point [C] was0.08%~0. 12%,[P]≤0.012% and [S]≤0.03%, and the yield of recarburizer was 85%~90%. During refining the basicity of slag was 2.5~3.0 with feeding Si-Ca wire and argon stirring. During concasting the temperature of liquid steel in tundish was 1495~1515 ℃, the casting speed 1.6~1.8 m/min using mold electromagnetic stirring. The quality experiment results of 20 heats 65Mn steel showed that the analyses of steel were C 0.63~0.68 ,Mn 0.95~1.07,P0.009~0.023,S0.006~0.017, and the deviation of carbon content at section of casting billet was ≤0.02%.The coil products of 65Mn steel met the requirements of standard GB/T4354- 1994.

摘要: 采用100t 顶底复吹转炉-100t 钢包炉(LF)精炼-6机6流150mm×150mm方坯连铸机生产65Mn  弹簧钢。转炉终点[C]0.08%~0.12%,[P]≤0.012%,[S]≤0.03%,增碳剂收得率为85%~90%。 LF精炼渣 碱度2.5~3.0,并喂Si-Ca线和吹氩。连铸时中间包钢水温度1495~1515℃,铸速1.6~1.8m/min,采用结晶 器电磁搅拌。20炉65Mn钢质量检验结果表明,化学成分(%):C0.63~0.68,Mn 0.95~1.07,P0.009~0.023, S0.006~0.017,连铸坯断面碳含量偏差≤0.02%C。65Mn钢盘条产品符合GB/T4354-1994要求。