Prediction of Austenite Recrystallized Grain Size in Hot Rolled Strip of C-Mn Steel

Li Zhuang, Zhou Xiaoguang, Wang Jiafu , Wu Di, Zhang Pingli   

  1. Northeastern University, Shenyang 110004
    Liaoning Provincial Education Department, Shenyang 110032
  • Received:2004-08-24 Online:2005-02-01 Published:2023-05-24

C-Mn钢热轧带奥氏体再结晶晶粒尺寸的预测

李壮,周晓光,王佳夫,吴迪,张平礼   

  1. 东北大学,沈阳110004
    辽宁省教育厅,沈阳110032
  • 作者简介:李 壮,男,40岁,副教授.博士研究生。工作单位:沈阳 航空工业学院,邮编110034, 1986年毕业于吉林工业大 学,从事金属材料的组织与性能研究“
  • 基金资助:
    国家自然科学基金资助项目{批准号: 50334010)

Abstract: Based on the research on physical metallurgy prediction model including the model of austenite recrystallization in microstructure evolvement, carbo-nitride precipitation, and relation between austenite phase transformation and structure-properties during strip control rolling and cooling, the austenite grain size of 0.16C-0.06Si-l.30Mn steel simulated calculated by computer after 7 pass hot deformation between 1 173 K and 1 081 K by Gleeble-1500 hot simulator was 43μm, mile the actual-measured austenite grain size in structure of strip after 7 pass deformation was 38 μm,the relative error was 13% . Therefore the austenite recrystallization grain size simulated calculated by computer better conform to that of actual measured value.

摘要: 在研究板带控轧控冷过程中钢中显微组织演变过程奥氏体再结晶、碳氮化合物析出、奥氏体相变和组织性能对应关系的物理冶金模型的基础上 ,通过Gleeble 15 0 0热模拟机和计算机模拟计算得出成分(% ) 0 16C ,0 0 6Si,1 30Mn钢在 1173~ 10 81K经 7道次热变形后奥氏体晶粒尺寸为 4 3μm ,同时实测 7道次变形后轧钢组织中奥氏体尺寸为 38μm ,相对误差 13%。计算机模拟计算的奥氏体再结晶晶粒尺寸与实测结果吻合较好。