Abstract: The experiment of commercial heat treatment process for 82 mm plate of steel 14Cr1MoR (0. 15C- 1.48Cr- 0.57Mo)has been carried out at Wuyang Iron and Steel. The test results showed that heat- treated with 9℃/min heating up speed, austenite conditioning at 930 ℃ for 2.4 min/mm,water quenching at 870 ℃,and tempering at 680 ℃ for 3.0 min/mm, air cooling,the structure of steel was sorbite, of which the ambient tensile strength was 590~650 MPa, yield strength 445~485 MPa,elongation 27%~28%,reduction of area 73%~75%,cross impact energy 173~212 J, and the Qo.z at 580℃ was 295~330 MPa. The properties of different parts of plate were uniform up to the requirement of stan- dard.
摘要: 在舞钢进行了82mm 厚14Cr1MoR(%:0. 15C,1.48Cr,0.57Mo)钢板的工业性热处理工艺试验。 试验结果表明,采用9℃/min速度加热,930℃奥氏体化2.4 min/mm,870℃水淬,680℃保温3.0 min/mm回火、 空冷、热处理后,钢的组织为索氏体,室温抗拉强度590~650 MPa,屈服强度445~485 MPa,延伸率27%~28%,断面收缩率73%~75%,20℃横向冲击功173~212 J,580℃co₂为295~330 MPa。钢板各部分性能均匀,满足标准要求。
关键词: 14CrlMo钢, 厚板, 热处理工艺
Yang Hailin, Yang Xiuqin. Experiment of Commercial Heat Treatment Process for 82 mm Plate of Steel 14Cr1MoR[J]. Special Steel, 2005, 26(3): 48-50.
杨海林, 杨秀芹. 82mm 14Cr1MoR钢板工业性热处理工艺试验[J]. 特殊钢, 2005, 26(3): 48-50.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2005/V26/I3/48